Concrete Discoloration: Drying Different Colors or Spotty - Concrete Network (2024)

Learn the common causes of concrete drying different colors or with spots and what countermeasures to take to fix the problemBy George Seegebrecht
Updated August 26, 2020

Some discoloration problems are baffling. These driveway lanes were placed on two different days with the same supplier, same mix, same crew, same subgrade, but with very different results.

Any contractor who has placed concrete that ends up being discolored knows how big of a nuisance and disappoint it can be to everyone involved. The contractor worked hard to deliver a product that reflects well on the company's image. The owner was looking forward to (and paid for) an attractive driveway, sidewalk, or patio that complements their home or commercial structure.

But when the concrete turns out to be blotchy and uneven in color, and takes away from rather than enhances a property's curb appeal, everyone wants to know why the discoloration happened and how it might be avoided or corrected.

Find concrete coloring contractors near me who can help fix discoloration.

COMMON CAUSES OF DISCOLORED CONCRETE

Discoloration is a tricky subject, since many factors can contribute to the problem (see photo). However, discoloration, whether occurring in a single placement or sequential concrete placements, generally boils down to one root cause: inconsistency. This can be an inconsistency in materials or in workmanship. Here are some of the most common causes and practices leading to discoloration and some remedies you can take to lessen the effects.

Inconsistent materials

To avoid objectionable color issues, it's important to maintain consistency throughout the project, especially in mix proportioning. Deliveries of mixes that are drastically different from batch to batch make it difficult to achieve a uniform concrete surface color.

It is the responsibility of your ready-mix producer to deliver a consistent concrete mix. But that's more complex than it sounds since concrete is made up of a number of ingredients with their own inherent variability. Cement, supplementary cementitious materials, sand, stone, water, admixtures, and possibly fibers are all blended together, and having them interact consistently from batch to batch does not happen "by accident." All concrete ingredients must comply with American Society for Testing and Materials (ASTM) standards. Concrete aggregates must be of good quality. Mix water quantities must be adjusted based on the moisture contents of the sand and stone. If not, the consequences in the field can be significant.

The lower portion of this driveway was placed with a mix containing calcium chloride, resulting in a darker color than the calcium-chloride-free placement near the garage door. (Photo courtesy of the Portland Cement Association)

Adding water at the jobsite

Sometimes contractors will adjust batches with inconsistent moisture contents (which translate to workability) at the jobsite to make finishing operations as easy as practical. Small variations in concrete moisture are common and typically not objectionable. But modifying mixes in the field, followed by inefficient mixing, can produce a blotchy appearance. Changes in shade become especially noticeable in side-by-side placements, when water is added in the field at the very end of one batch and then the concrete is placed next to earlier non-retempered concrete.

RELATED: Guide to Efflorescence on Concrete

Change in cement color

Cement delivered to the ready-mix plant may change slightly in color depending on the burning or grinding conditions during cement production. A concrete color change, due to a change in cement color, may be noticeable if a cement substitution takes place during an ongoing placement or this adjusted mix is placed immediately next to concrete produced with cement from a different source.

Avoid adding water to the surface as a finishing aid or finishing the bleedwater back into the surface. Higher water-cement ratios lead to lighter-colored concrete surfaces. (Photo courtesy of PCA)

Using cement replacements

To complicate the color issue, the trend to go "green" and use recycled products as partial cement replacements can produce color variations, depending on the percentage of recycled material put into the mix, the water-to-cementitious materials ratio, and how the concrete is cured. Common recycled or supplemental cementitious materials (SCM) are slag, a byproduct of the steel industry, and fly ash, a byproduct of coal combustion. Using varying quantities of fly ash can result in different hues, ranging from buff to brown. Slag use may produce an initial slight bluish or green tint that lightens with time. Generally, a slag-cement mix will be lighter than a straight-cement concrete.

Adding calcium chloride

A frequent reason behind a darkened-concrete appearance is the addition of calcium chloride to accelerate the setting time of concrete (see Photo 1), especially when calcium chloride dosages approach 2% by weight of cement. Inadequate mixing after addition of calcium chloride makes the concrete color even more irregular or blotchy.

Poor workmanship

How a contractor reacts to variables during a concrete placement, such as weather conditions that change from morning to afternoon and day to day, can have a big impact on the final results. For instance, in a dry environment, wetting down a subgrade prior to a slab placement is good practice. Placed concrete in weather producing higher rates of evaporation may also call for countermeasures such as wind breaks, evaporative retardants or similar practices (for more information, read the American Concrete Institute publication ACI 305R-20, Hot Weather Concreting). Without proper countermeasures, poor practices like "blessing" the surface with additional water (see Photo 2) or final finishing while bleedwater is still on the surface result in increased variability in the surface appearance or, worse, delamination.

HOW DO YOU FIX DISCOLORED CONCRETE?

If you do end up with discolored concrete, there are a number of remedies you can take to lessen the effects.

Check out these top color correction resources:

  • Fixing Discolored Concrete Floors
  • How to Fix Concrete Color Issues
  • Removing Stains from Concrete
  • Concrete Sealer Issues

Shop for Related Products

Concrete Discoloration: Drying Different Colors or Spotty - Concrete Network (4)Efflorescence CleanerWater soluble formula safe for indoor use.

Concrete Discoloration: Drying Different Colors or Spotty - Concrete Network (5)Thin Micro-ToppingProduces durable surface to color or stain

Concrete Discoloration: Drying Different Colors or Spotty - Concrete Network (6)Cleaner & DegreaserStarting at $10.95

Concrete Discoloration: Drying Different Colors or Spotty - Concrete Network (7)Colored Outdoor SealerAcrylic specifically formulated for UV stability


Start by trying these simple solutions:

First, flush the hardened surface with hot water, followed by scrubbing with a stiff brush. This process should be repeated until discoloration disappears. Learn more about cleaning colored concrete.

For more severe discoloration, try using a mild acid solution (1% to 3% muriatic acid) Start with a mild concentration, since muriatic acid will remove concrete as the concentration increases. Use just enough to remove the discoloration. To control the depth of acid penetration, flood the hardened surface with water first, and allow it to dry. The longer you allow the concrete to dry, the deeper the acid can penetrate. Work in manageable areas, and control the depth of acid penetration according to the drying time following flooding.

After each attempt with the mild acid, flush the area completely with clean water within 15 minutes after acid application. As when using any aggressive chemical, refer to the materials safety data sheet (MSDS) and wear appropriate clothing and eye protection.

If you can't fix the discoloration with the above methods, you may have success using these:

  • Tinted concrete sealer
  • Concrete paint
  • Concrete resurfacing

PREVENTING UNWANTED COLOR VARIATIONS IN CONCRETE

Here are a few things contractors can do to reduce or prevent excessive or unacceptable color variations in their concrete placements:

Swipe to view slides

  • Avoid excessive troweling of an exterior concrete surface. Densification of the concrete surface darkens concrete color by reducing the water-to-cementitious materials ratio.

  • Using wall forms with different degrees of wear and absorbency can result in color variations. Form materials with higher absorbency will reduce the surface water-cement ratio, resulting in a darker appearance.

  • To minimize discoloration, polyethylene sheeting should be placed flat on the concrete surface. (Photo courtesy of PCA)

  • When penetrations or other obstacles prevent flat placement of plastic sheeting, impressions are left where the plastic created a green house effect. (Photo courtesy of PCA)

  • Clearly communicate with the owner or their representative concerning acceptable surface appearance. Construct a mockup that is left onsite or cast in a noncritical area to serve as an onsite "referee" to settle any misunderstandings. Use the identical mix intended for the work as well as the same placement method, forms, crew and curing method for your mockup. Shortcuts here will usually cause problems later.

  • Establish early communications with the batch plant concerning mix performance to avoid the need to make less accurate adjustments in the field. If color is a priority, the mix should be delivered from the same plant for the entire placement.

  • Prepare a uniform subgrade, and moisten the subgrade uniformly prior to concrete placement (but remove any standing water).

  • For exterior flatwork, properly time final finishing operations and wait until all bleedwater has dissipated. Do not broadcast cement on the surface to accelerate this process, since this practice will commonly lead to discoloration.

  • Avoid hard troweling exterior concrete. Not only can hard troweling reduce the air content of the concrete surface, making it less durable in freeze-thaw environments, it can also darken the concrete because it densifies the surface (see Photo 3).

  • For vertical concrete work, use forms that are in good condition and won't absorb water or leak around the edges. Color differences may also occur when older forms are used immediately adjacent to concrete placed in new forms (see Photo 4). If you plan to use new forms, consult with the form manufacturer and prepare a mockup to establish standards for project acceptance.

  • Clean forms thoroughly before use, and apply an even coat of form release oil to form faces in contact with concrete.

  • Don't use calcium chloride in nonreinforced concrete when color and appearance are important.

  • Cure the concrete uniformly over the entire surface. The best methods include wet curing with tepid water (at a temperature difference of no more than 20° F from the new concrete), proper application of a liquid curing compound, leaving forms in place, or by covering with polyethylene sheeting kept in uniform contact with the slab surface (see Photos 5 and 6).

References:

"Discoloration of Concrete, Causes and Remedies," Kosmatka, S.H., Concrete Products Magazine, April 1987.

"Effects of Substances on Concrete and Guide to Protective Treatments," Beatrix Kerkhoff, Publication IS 001.11, Portland Cement Association, 2007.

Concrete Discoloration: Drying Different Colors or Spotty - Concrete Network (2024)

FAQs

Concrete Discoloration: Drying Different Colors or Spotty - Concrete Network? ›

Factors influencing the discoloration are calcium chloride mixtures, cement alkalis, hard surfaces, inadequate or insufficient curing, wet subsurface, varying proportions of aqueous cement on the surface, and changes in the concrete mixture. Discoloration from these causes appears very soon after concreting.

Why is my concrete drying spotty? ›

But if the sealer isn't applied uniformly to begin with, or if not enough coats are used, the slab will appear blotchy upon drying. This is caused by the sealer filling in some of the valleys, but not all, and failing to remain on top of the hills.

How do you fix blotchy concrete stain? ›

Cover the Stain With Concrete Paint

Undoubtedly, the easiest and most common way to solve a botched concrete staining job is to just cover it up. This option will involve preparing the surface to accept a new finish and then applying it.

Does concrete dry spotted? ›

The resulting color of the surface is very dependent on the amount of moisture and the curing/drying conditions of the slab. These conditions lead to areas of higher and lower water-cement ratios, with the result ending in dark spots (thin mortar coverage...

What makes concrete different colors? ›

The higher the water content of the mix, the lighter the color. Control of the water/cement ratio is vital for consistent color from batch to batch. These are factors beyond the pigment that can play a role in the final appearance of the product.

Why is my concrete drying different colors? ›

Factors influencing the discoloration are calcium chloride mixtures, cement alkalis, hard surfaces, inadequate or insufficient curing, wet subsurface, varying proportions of aqueous cement on the surface, and changes in the concrete mixture. Discoloration from these causes appears very soon after concreting.

What is mottled concrete? ›

Mottled concrete is irregular shapes of different shades of white- gray to gray-black. These blotches are restricted to the surface, normally only 1/32" to 1/8" deep. They can diminish over time but usually are permanent.

Will my concrete dry the same color? ›

If the concrete can cure consistently, the end result is usually a quality concrete product with consistent color and finish. If a foreign object retards the movement of moisture out of the concrete or traps moisture at the surface, a curing differential occurs, resulting in a color shift in the concrete surface.

How do you clean Discoloured concrete? ›

Vinegar or baking soda: These natural cleaners work well to clean cement patios with stubborn charcoal or rust spots. Mix equal parts vinegar and water, scrub the patio with the mixture, then give it a good rinse. If stains don't dissolve, try undiluted vinegar.

Can you reverse stained concrete? ›

A small amount of acid added to the water will pull the stain out of the concrete without etching the concrete surface. In essence, the acidic solution reverses the reaction, allowing you to pull the color back out of the concrete.

What happens if you put too much sealer on concrete? ›

Sealer that is applied too heavily or too often will create an impermeable barrier and trap that water vapor beneath it. If enough pressure is created by trapped water vapor, the sealer can delaminate from the concrete surface, and might even take some of the concrete paste with it!

What are the dark brown spots on concrete? ›

For example, new concrete turning brown may be caused by excessive mineral or iron content. To fix this, an acid rinse or heated pressure cleaning will work. Post-cleaning sealing might also be necessary if discoloration reoccurs.

Does concrete get lighter as it dries? ›

Fresh concrete is always much darker than when it is fully cured and dry. Even uncolored concrete. Wait at least 7 to 10 days until the new concrete has hardened and dried. If the concrete is on a wet subgrade or there's underground water, it may stay dark for as long as it's wet.

What are the blemishes on concrete? ›

When a blemish appears on the surface of a concrete slab it will likely be one of these: blisters, cracking, crazing, curling, delamination, discol- oration, dusting, efflorescence, low spots, popouts, scaling, or spalling.

Why is my concrete blotchy after pressure washing? ›

If you notice dark spots on concrete after pressure washing, it's likely that the surface is damaged and that the top layer is washed off. This type of damage is prevalent in slabs that are topped with a screed with a different color from the base concrete.

Should you spray water on drying concrete? ›

Properly curing your concrete improves strength, durability, water tightness, and resistance for many years. The first 7 days after installation you should spray the slab with water 5-10 times per day, or as often as possible. Once the concrete is poured the curing process begins immediately.

What happens if there is too much moisture in concrete? ›

Excess moisture in the concrete slab can cause serious flooring problems, such as adhesive failure, discolored tile or grout, bubbles in sheet vinyl, and buckling of wood floors.

Top Articles
Latest Posts
Article information

Author: Francesca Jacobs Ret

Last Updated:

Views: 5561

Rating: 4.8 / 5 (48 voted)

Reviews: 87% of readers found this page helpful

Author information

Name: Francesca Jacobs Ret

Birthday: 1996-12-09

Address: Apt. 141 1406 Mitch Summit, New Teganshire, UT 82655-0699

Phone: +2296092334654

Job: Technology Architect

Hobby: Snowboarding, Scouting, Foreign language learning, Dowsing, Baton twirling, Sculpting, Cabaret

Introduction: My name is Francesca Jacobs Ret, I am a innocent, super, beautiful, charming, lucky, gentle, clever person who loves writing and wants to share my knowledge and understanding with you.